Surface passivation model explains pyrite oxidation kinetics in column experiments with up to 11 bars p(O2).
Berta, M., Dethlefsen, Frank, Ebert, Markus, Gundske, K. and Dahmke, Andreas (2016) Surface passivation model explains pyrite oxidation kinetics in column experiments with up to 11 bars p(O2). Environmental Earth Sciences, 75 (16). DOI 10.1007/s12665-016-5985-7.
Full text not available from this repository.Abstract
Despite decades of research in numerous experimental and field studies, the reaction kinetics of pyrite oxidation is still not characterized for high partial pressures of oxygen and near-neutral pH-levels. These conditions potentially exist in aquifers where oxidative site remediation, temporary water storage, or a leakage from a compressed air energy storage facility is present. For planning and monitoring of such field operations, their potential side effects on protected natural resources like groundwater have to be characterized. Thereby, site-scale assessments of such side effects of subsurface use by numerically modeling geochemical changes caused by the presence of oxygen need parametrization. Also, a function transferring results from simple, low pressure experiments to high pressure environments requires experimental bases. Pyrite oxidation can be the main consequence of oxygen intruding reduced aquifers. In this study, pyrite oxidation kinetics was examined at oxygen partial pressures from 0 to 11 bars, corresponding to an air intrusion in up to 500 m depth, at neutral pH-levels in high and low pressure flow-through column experiments representing aquifer conditions. A reaction rate equation was developed and evaluated with 1D PHREEQC numerical reactive transport models using experimental data as transfer function between high pressure and low pressure experiments. This model development included an improvement of established rate laws with a passivation term, which is, in contrast to previously published functions, dependent on the partial pressure of oxygen. The resulting model on passivated oxidation kinetics of pyrite at high oxygen partial pressures was able to reproduce independent experimental results acquired using different experimental set-ups. This assessment found the passivation to overcome the theoretical increase in pyrite oxidation kinetics caused by elevating oxygen partial pressure. These findings contribute to future experimental and modeling efforts for risk assessment and monitoring of oxygen-rich plumes in the subsurface.
Document Type: | Article |
---|---|
Additional Information: | Times Cited: 0 Berta, Marton Dethlefsen, Frank Ebert, Markus Gundske, Karsten Dahmke, Andreas |
Keywords: | Compressed air energy storage Pyrite oxidation kinetics Column experiments High pressure oxygen measurement Air in aquifer Surface passivation Air leakage ANGUS+ |
Research affiliation: | OceanRep > The Future Ocean - Cluster of Excellence Kiel University |
Refereed: | Yes |
Open Access Journal?: | No |
Publisher: | American Medical Association |
Projects: | Future Ocean |
Date Deposited: | 18 Mar 2017 11:48 |
Last Modified: | 20 May 2019 12:20 |
URI: | https://oceanrep.geomar.de/id/eprint/36012 |
Actions (login required)
View Item |
Copyright 2023 | GEOMAR Helmholtz-Zentrum für Ozeanforschung Kiel | All rights reserved
Questions, comments and suggestions regarding the GEOMAR repository are welcomed
at bibliotheksleitung@geomar.de !